MICRO—FINE
1700
Casting Investment
FAST – ACCURATE & FORGIVING
HERE’S WHY
| |
EVERY BODY
ELSE |
|
TALLADIUM, INC. |
|
-
Investments set time 45 minutes
|
|
- 15 minutes
(at room temperature 72°F)
|
- Rapid
Burnout Investments-1600°F with at least 2 rings. This is to lower
entry shock.
|
|
- 1700°F
entry temperature on a single ring or more. It doesn’t matter with
ours!!
|
- Rapid
Burnout turn around time, wax pattern to metal-2 hours
|
|
- 30
MINUTES. This represents a 100% savings!!!
|
MICRO—FINE 1700 CASTING INVESTMENT could be the first of a new
generation of Pure Ceramic Investments that replaces the old ground
sand-phosphate type of investments. Because of its precision computer
controlled particles size distribution, we are able to give the laboratory not
only a perfect fit in larger bridges time after time; but an “incredible
expansion” Investment on the market today! This means you can dial in your fit.
Because TALLADIUM does all in house manufacturing of its product, you are
receiving fresh quality controlled batches. Most companies will give you a
perfect range to work with. We give you a precise measurement on what to use on
all metals. Crown and Bridge Gold, Semi-precious and Base Metals. “Batch
customized measurements” are figured out on each batch manufactured by having a
technician wax to a die, cast and judge the fit. Then a bulletin is generated
by computer for that particular batch to take the guesswork out of the
laboratory.

|
|